保定钻铤
标准:API SPEC 7-1
钢种:AISI 4145H
尺寸:3 1/8" -- 11"
连接类型:NC、IF、REG
类别:
保定油井管
电话:400-888-8888
产品描述
API SPEC 7-1钻铤由轧制或锻造AISI4145H铬钼合金钢制成。因此,需要有效控制化学成分和微量元素的含量。

|
标准 |
数字 |
外径 |
内径 |
长度 |
重量 |
典型的抗弯 |
|
SY5144-2007/API7-1 |
NC 23-31 |
3-1/8 |
1-1/4 |
30 |
22 |
2.57:1 |
|
NC 26-35 (2-3/8 IF) |
3-1/2 |
1-1/2 |
30 |
27 |
2.42:1 |
|
|
NC 31-41 (2-7/8 IF) |
4-1/8 |
2 |
30 or 31 |
34 |
2.43:1 |
|
|
NC 35-47 |
4-3 /4 |
2 |
30 or 31 |
47 |
2.58:1 |
|
|
NC 38-50 (3-1/2 IF) |
5 |
2-1/4 |
30 or 31 |
54 |
2.38:1 |
|
|
NC 44-60 |
6 |
2-1/4 |
30 or 31 |
83 |
2.49:1 |
|
|
NC 44-60 |
6 |
2-13 /16 |
30 or 31 |
76 |
2.84:1 |
|
|
NC 44-62 |
6-1/4 |
2-1/4 |
30 or 31 |
91 |
2.91:1 |
|
|
NC 46-62 (4 IF) |
6-1/4 |
2-13 /16 |
30 or 31 |
84 |
2.63:1 |
|
|
NC 46-65 (4 IF) |
6-1/2 |
2-1/4 |
30 or 31 |
100 |
2.76:1 |
|
|
NC 46-65 (4 IF) |
6-1/2 |
2-13 /16 |
30 or 31 |
93 |
3.05:1 |
|
|
NC 46-67 (4 IF) |
6-3 /4 |
2-1/4 |
30 or 31 |
109 |
3.18:1 |
|
|
NC 50-70 (4-1/2 IF) |
7 |
2-1/4 |
30 or 31 |
118 |
2.54:1 |
|
|
NC 50-70 (4-1/2 IF) |
7 |
2-13 /16 |
30 or 31 |
111 |
2.73:1 |
|
|
NC 50-72 (4-1/2 IF) |
7-1/4 |
2-13 /16 |
30 or 31 |
120 |
3.12:1 |
|
|
NC 56-77 |
7-3 /4 |
2-13 /16 |
30 or 31 |
140 |
2.70:1 |
|
|
NC 56-80 |
8 |
2-13 /16 |
30 or 31 |
151 |
3.02:1 |
|
|
6-5/8 API Reg |
8-1/4 |
2-13 /16 |
30 or 31 |
162 |
2.93:1 |
|
|
NC 61-90 |
9 |
2-13 /16 |
30 or 31 |
196 |
3.17:1 |
|
|
7-5/8 API Reg |
9-1/2 |
3 |
30 or 31 |
217 |
2.81:1 |
|
|
NC 70-97 |
9-3 /4 |
3 |
30 or 31 |
230 |
2.57:1 |
|
|
NC 70-100 |
10 |
3 |
30 or 31 |
243 |
2.81:1 |
|
|
8-5/8 API Reg |
11 |
3 |
30 or 31 |
300 |
2.84:1 |
| 卷标 |
化学成分 % |
||||||||
|
C |
Si |
Mn |
P |
S |
Cr |
Mo |
Cu |
Al |
|
|
4145H |
0.42~0.48 |
0.15~0.35 |
0.90~1.20 |
≤0.03 |
≤0.03 |
0.90~1.20 |
0.15~0.25 |
≤0.2 |
0.025~0.045 |
|
其他元素:N≤0.015,Ni≤0.5 |
|||||||||
|
钻铤机械性能 |
||||||||
|
钻铤外径范围 |
屈服强度 |
抗拉强度 |
伸长率 |
|
冲击t |
|||
|
mm |
in |
MPa |
Psi |
MPa |
Psi |
|||
|
79.4~171.4 |
3-1/8~6-3/4 |
≥758 |
≥110000 |
≥965 |
≥140000 |
≥13 |
285~341 |
≥54 |
|
177.8~279.4 |
7~11 |
≥689 |
≥100000 |
≥930 |
≥135000 |
≥13 |
285~341 |
≥54 |
|
特殊条件下,夏比冲击功可根据供求关系确定为大于70J |
||||||||
过程
钻铤在热处理过程中增加了特殊的正火工艺,使螺纹部分晶粒更加细化,增强了钻铤螺纹强度,有效提高了钻铤的使用寿命。